HomeEngineeringOther parameters remaining same, the recrystallisation temperature of an alloy is lowered, when 847. Other parameters remaining same, the recrystallisation temperature of an alloy is lowered, whenBy Admin / September 6, 2025 A. Strain rate is increased B. Grain size is increased C. Prior cold deformation is increased D. Not affected by any of the above parameters ✅ The correct answer is option A.