17007. The temperature required for full annealing in hyper-eutectoid steel is

30° C to 50° C above upper critical temperature
30° C to 50° C below upper critical temperature
30° C to 50° C above lower critical temperature
30° C to 50° C below l
✅ The correct answer is option C.